I have a 360 gallon acrylic tank and the seams are pretty nice minus a few spots where on the inside edges of the seams its as if about 1/16 inch of the seam has been whited out and in one spot the seam i whited out pretty bad how do i fix this? Do i get weld on 4 or 16 and apply it on the seams or do i weld on 1/4x1/4 rod on every seam? SOrry no pics but the main question here is what to do about white seams?